  • Carefully remove the substrate from the sample holder.
  • Place the substrate in a developer bath (PGMEA for most resins, methanol for GP-Silica) to wash away excess liquid 2PP resin.
  • Leave substrate in developer at least 15 minutes, high aspect ratio structures require additional development time.
  • Wash away the developer with IPA.
  • Transfer to IPA for at least 15 minutes.Gently blow-dry the sample (Optional- dependent on size and strength of your structure, use with extreme caution).
  • Cure remaining liquid 2PP resin if a shell and scaffold structure was printed.

...